Skip to main content

A synergistic hydro- and pyrometallurgical approach for the effective metal recovery from Waelz slag

In the quest to develop new waste-to-resource pathways for industrial residues, this work aims to recover iron from Waelz slag (WS), the main residue of electric arc furnace dust processing in the Waelz process, using a combined hydrometallurgical and pyrometallurgical process. WS was pre-treated via alkaline leaching using a 6M NaOH solution, which was designed to extract those undesirable elements (e.g., Zn, S, and Pb) from both the perspective of metallurgical quality of the recovered iron and the yield of pyrometallurgical processing. Hydrometallurgical alkaline leaching pretreatment removed over 60 wt.% of Zn and over 45 wt.% of Pb and S while preserving over 95 wt.% of the initial Fe content. The solid residue was then subjected to carbothermic reduction at 1500 °C and the characteristics of the reduction products were compared to those achieved by the reduction products of an untreated WS. Regardless of the hydrometallurgical pre-treatment, the reduction product consisted of an interconnected matrix of metallic iron and secondary slag. Nevertheless, alkaline leaching had a beneficial effect on the amount of metallic iron in the reduction products of the pre-treated WS. They contained up to two times more the amount of iron (19.78-23.34 wt.% vs. 9.52 wt.%), with a metallization degree higher than 95 wt.%. Furthermore, the decrease in undesirable elements associated with alkaline leaching made the reduction products of the pre-treated WS more suitable to be considered as a secondary iron source for metallurgical furnaces, thereby opening new valorization routes for the WS.

Details

Author
Gianluca Dall'Osto1, Davide Mombelli1, Sara Scolari1, Carlo Mapelli1
Institutionen
1Politecnico di Milano, Italy
Veranstaltung
GeoMinBochum 2026
Datum
2026
DOI
10.48380/m169-v354